1. Engineering
  2. Chemical Engineering
  3. a carburizing process is carried out on a 010c steel...

Question: a carburizing process is carried out on a 010c steel...

Question details

A carburizing process is carried out on a 0.10%C Steel by introducing 1.10%C at the surface at 950°C, where the iron is FCC. Calculate the carbon content at 0.5 cm beneath the surface after 2 h.

Q=32,900cal/mol

Do=0.23cm2/s.

0.0 0.000 1.0 0.843 0.1 0.1121.10.880 0.2 0.223 1.2 0.910 0.3 0.329 1.3 0.934 0.4 0.428 1.4 0.952 0.5 0.520 1.5 0.966 0.7 0.6