1. Engineering
  2. Mechanical Engineering
  3. problem 2 compare the experimental results of e2 for different...

Question: problem 2 compare the experimental results of e2 for different...

Question details

Problem 2: Compare the experimental results of E2 for different fiber volume fraction from study by Tsai (results shown in the figure below) with predicted values by iso-strain, iso-stress and self-consistent field micromechanical models. Use the following material properties for fiber and matrix: Er - 10.6. 106 psi, v0.22, E05 106 psi, vm0.35. How do different models compare with experimental results? -2 yt-1 14 Hashin (ub) 3 20 Hashin (b 10 0 0.4 Fiber volume ratio, V 0.2 0.6 0.8